Castadur-50

Castadur-50 / AlZn5Mg (RHEINFELDEN ALLOYS) | Sand casting

Manufacturer-reported values. Do not use as certified design allowables. View sources ↗

TemperWallYield MPaTensile MPaElong. %
T1Not specified160–200220–2805–10

T1 condition: Original-supplier T1 self-aged performance range. Wall thickness, test specimen size, test temperature and precise ageing duration are not reported for this row.

Chemical composition

Only reviewed weight-percent bounds are listed. A blank bound means only the other threshold was reported.

Original-supplier branded Castadur-50 / AlZn5Mg, not generic AlZn5Mg. The 2015 overview, 2016 handbook, REACH technical information and current product page are one issuer, not independent votes. The T1 sand-cast mechanical row does not state wall thickness, specimen size, test temperature or precise self-ageing duration. The F application sheet is a cover page with no numerical table; it does not establish F-state mechanical values. Blank gravity-die shrinkage and fatigue cells remain absent. REACH ingredient-disclosure ranges are not ingot specification limits.

Element / source labelMinimum wt%Upper wt%
Si—0.15
Fe—0.2
Cu—0.05
Mn0.10.2
Mg0.40.8
Zn4.95.8
Ti—0.15
Cr0.20.4

Physical and thermal properties

PropertyReported valueUnitCondition
density2.78kg/dm³Supplier physical summary; heat-treatable alloy in heat-treated state; test temperature not separately reported
youngs modulus71–74GPaSupplier physical summary; heat-treatable alloy in heat-treated state; test temperature not separately reported
thermal expansion2410⁻⁶/KSupplier physical summary; heat-treatable alloy in heat-treated state; 20–200 °C
thermal conductivity1.3W/(K·cm)Supplier physical summary; heat-treatable alloy in heat-treated state; 20–200 °C
electrical conductivity18–21MS/mSupplier physical summary; heat-treatable alloy in heat-treated state; MS/m; temperature not separately reported
electrical conductivity31–36%IACSSupplier physical summary; heat-treatable alloy in heat-treated state; %IACS; temperature not separately reported
linear shrinkage1.0–1.4%Supplier physical summary; heat-treatable alloy in heat-treated state; sand casting; temperature not separately reported
melt solidification range555–655°CSupplier melt and solidification range; includes partial-melting onset from segregation in cast structure
density2.78g/cm³Manufacturer REACH technical information, 2015 version 2; stated at 20 °C; product form not further specified
melting range555–655°CManufacturer REACH technical information, 2015 version 2; modification state and measurement method not stated

Additional property data

Source-reported values, specification intervals, minimums and strict bounds; an average is labeled only when the source reports it. Compare conditions before use.

PropertyValueCondition
brinell hardness75–85 HBWSand casting; T1 self-aged; supplier performance range; wall thickness not reported
ignition temperature400 °CManufacturer REACH technical information; dust form only; not a bulk-alloy ignition temperature

Evidence

Castadur-50 original-supplier handbook (2016) — RHEINFELDEN ALLOYS GmbH & Co. KG

Castadur-50 original-supplier overview (2015) — RHEINFELDEN ALLOYS GmbH & Co. KG

Castadur-50 original-supplier tdb (2015) — RHEINFELDEN ALLOYS GmbH & Co. KG

Show the exact source location for each value